| ◎ 产品展示 |
 |
| 耐火缓冲泥浆 |
| |
|
项目 指标 |
HCN-L |
HCN-G1 |
HCN-G2 |
FHCN-TG |
| AL2O3,% |
≥70 |
/ |
/ |
/ |
|
SiO2,% |
/ |
≥80 |
≥70 |
/ |
|
SiC,% |
/ |
/ |
/ |
≥50 |
| 耐压强度,MPa |
110℃×16h |
≥0.5 |
≥0.5 |
≥0.5 |
(200℃)≥1.0 |
| 1000℃×3h |
≥0.2 |
500℃×3h≥0.5 |
/ |
≥0.25 |
| 烧后线收缩率,% |
1000℃×3h≤1.0 |
500℃×3h≤1.0 |
800℃×3h≤1.0 |
1000℃×3h≤1.0 |
热态压缩率,% |
≥15 |
≥15 |
≥55 |
≥30 |
|
| |
|
|